YLF (Yttrium Lithium Fluoride) features weak thermal lensing, large fluorescence linewidth and naturally polarized oscillation. Using Czochralski technique, LNG Optics provide Nd:YLF, Ho:YLF, Tm:YLF and Pr:YLF with different doping rates. We also accept contract growth of special doped YLF crystals according to customers’ requirements.
Laser Gain Properties:
|
Nd:YLF
|
Tm:YLF
|
Ho:YLF
|
Pr:YLF
|
Lasing action
|
4 level
|
Quasi 3 level
|
3 level
|
4 level
|
Current dopant level in LNG (at%)
|
0.5 – 1.1
|
2 & 3
|
|
0.5
|
Lasing wavelength (nm)
|
1047&1053/4F3/2→4I11/2
|
1900/3F4→3H6
|
2050/5I7→5I8
|
640/3P0→3F2
|
Stimulated Emission Cross-Section
(×10-20 cm2)
|
18 @ 1047nm
12 @ 1053nm
|
0.2
|
0.9
|
22
|
Spontaneous Fluorescent Lifetime (μs)
|
480 @ 1 at%
|
14000
|
15000
|
50
|
Refractive Index
|
no = 1.4481
ne = 1.4704
@ 1050nm
|
no = 1.448
ne = 1.470
@ 1064nm
|
no=1.448
ne=1.470 @ 1064nm
|
no=1.443
ne=1.464 @ 600nm
|
Pump wavelength (nm)
|
792
|
792
|
1940
|
444
|